核电站燃料包壳用含硫的锆铌铁合金

    公开(公告)号:CN103589910B

    公开(公告)日:2016-05-25

    申请号:CN201310398814.0

    申请日:2013-09-05

    Applicant: 上海大学

    CPC classification number: Y02E30/40

    Abstract: 本发明涉及一种能用作压水堆核电站燃料包壳以及定位格架条带等结构材料含硫的锆铌铁合金,属于锆合金材料技术领域。该锆合金的化学组成以重量百分比计为:0.5%~1.5%Nb,0.03%~0.5%Fe,0.0005%~0.06%S,余量为Zr。合金元素优选范围为:0.8%~1.0%Nb,0.07%~0.3%Fe,0.0015%~0.01% S或0.015%~0.06% S。本发明的锆合金在400℃/10.3 MPa过热蒸汽和360 ℃/18.6 MPa去离子水中表现出优良的耐腐蚀性能,明显优于Zr-1Nb合金,且加工性好,可在核电站压水堆中用作燃料元件包壳以及定位格架条带等堆芯结构材料。

    核电站燃料包壳用含铜含锗的锆合金

    公开(公告)号:CN103451473A

    公开(公告)日:2013-12-18

    申请号:CN201310389785.1

    申请日:2013-09-02

    Applicant: 上海大学

    CPC classification number: Y02E30/40

    Abstract: 本发明涉及核电站燃料包壳用含铜含锗的锆合金,属于锆合金技术领域。该锆合金的组成以重量百分比计为:(1)0%~1.5%Sn,0.2%~1.2%Nb,0.01%~0.4%Fe,0~0.3%Cr,0.01%~0.5%Cu,0.01%~0.8%Ge,余量为Zr;(2)0.3%~1.2%Sn,0.2%~1%Nb,0.05%~0.4%Fe,0.01%~0.4%Cu,0.01%~0.5%Ge,余量为Zr;(3)0.2%~1.2%Nb,0.01%~0.4%Fe,0.01%~0.5%Cu,0.01%~0.8%Ge,余量为Zr。本发明的锆合金在3种水化学条件下均表现出优良的耐腐蚀性能,优于Zr-0.7Sn-1Nb-0.2Fe合金,且加工性好,可在核电站压水堆中用作燃料元件包壳以及定位格架条带等堆芯结构材料。

    核反应堆燃料包壳用锆合金

    公开(公告)号:CN102230110A

    公开(公告)日:2011-11-02

    申请号:CN201110189363.0

    申请日:2011-07-07

    Applicant: 上海大学

    CPC classification number: Y02E30/40

    Abstract: 本发明涉及一种核反应堆燃料包壳用锆合金,属锆合金材料技术领域。该锆合金的化学组成以重量百分比计为:0.5%~0.9%Sn,0.3%~0.5%Fe,0.12%~0.3%Cr,0.1%~0.19%Nb,余量为Zr。本发明的锆合金在多种水化学条件下均表现出优良的耐腐蚀性能,明显优于我国研发的优化N18和N36合金,也优于已商用的Zr-4、ZIRLO、E635和E110锆合金,并且对热加工工艺过程中温度的变化不敏感,可在核反应堆压水堆和沸水堆中用作燃料元件包壳、格架等堆芯结构体的材料。

    一种耐超临界水腐蚀的锆合金材料

    公开(公告)号:CN1827813A

    公开(公告)日:2006-09-06

    申请号:CN200610025241.7

    申请日:2006-03-30

    Applicant: 上海大学

    Abstract: 本发明涉及一种耐超临界水腐蚀的锆合金材料,属特种合金材料配方及加工工艺技术领域。本发明的锆合金成分(重量百分含量)为:Zr 95.3~98.3%,Nb 1.5~3.5%,Cu 0.2~0.8%,Fe 0.05~0.4%,其余杂质含量符合目前核用锆合金的标准。该合金的制备过程和步骤如下:(1)用核级海绵锆和核级纯金属原料按上述配方配料并压制成电极,采用真空自耗电弧炉进行两次熔炼制成合金锭;(2)将合金锭在850~1050℃进行锻造加工或挤压制成坯材;再经1020~1050℃β相加热均匀化处理后淬火;(3)坯材经多次冷轧,并在低于600℃进行中间退火,制成板材或管材;最后制品经580℃再结晶退火处理,即制得一种耐超临界水腐蚀的锆合金材料。

    核电站燃料包壳用含铜含锗的锆合金

    公开(公告)号:CN103451473B

    公开(公告)日:2016-08-10

    申请号:CN201310389785.1

    申请日:2013-09-02

    Applicant: 上海大学

    CPC classification number: Y02E30/40

    Abstract: 本发明涉及核电站燃料包壳用含铜含锗的锆合金,属于锆合金技术领域。该锆合金的组成以重量百分比计为:(1)0%~1.5%Sn,0.2%~1.2%Nb,0.01%~0.4%Fe,0~0.3%Cr,0.01%~0.5%Cu,0.01%~0.8%Ge,余量为Zr;(2)0.3%~1.2%Sn,0.2%~1%Nb,0.05%~0.4%Fe,0.01%~0.4%Cu,0.01%~0.5%Ge,余量为Zr;(3)0.2%~1.2%Nb,0.01%~0.4%Fe,0.01%~0.5%Cu,0.01%~0.8%Ge,余量为Zr。本发明的锆合金在3种水化学条件下均表现出优良的耐腐蚀性能,优于Zr?0.7Sn?1Nb?0.2Fe合金,且加工性好,可在核电站压水堆中用作燃料元件包壳以及定位格架条带等堆芯结构材料。

    核电站燃料包壳用含锗铋的锆铌合金

    公开(公告)号:CN105400997A

    公开(公告)日:2016-03-16

    申请号:CN201510902368.1

    申请日:2015-12-09

    Applicant: 上海大学

    CPC classification number: Y02E30/40 C22C16/00 G21C3/07

    Abstract: 本发明涉及一种能用作压水堆核电站燃料包壳以及定位格架条带等结构材料含锗铋的锆铌合金,属于锆合金材料技术领域。该锆合金的化学组成以重量百分比计为:0.9%~1.1%Nb,0.01%~0.1%Ge,0.1%~0.6%Bi,余量为Zr。合金元素优选范围为:0.9%~1.1%Nb,0.03%~0.08%Ge,0.2%~0.4%Bi。本发明的锆合金在400℃/10.3MPa过热蒸汽和360℃/18.6MPa去离子水中表现出优良的耐腐蚀性能,明显优于Zr-1Nb合金,且加工性能良好,可在核电站压水堆中用作燃料元件包壳以及定位格架条带等堆芯结构材料。

    核电站燃料包壳用锆铌铜铋合金

    公开(公告)号:CN105018794A

    公开(公告)日:2015-11-04

    申请号:CN201510399305.9

    申请日:2015-07-09

    Applicant: 上海大学

    CPC classification number: Y02E30/40

    Abstract: 本发明涉及一种用作压水堆核电站燃料包壳以及定位格架条带等结构材料锆铌铜铋合金,属于锆合金材料技术领域。该锆合金的化学组成以重量百分比计为:0.7%~1.2%Nb,0.05%~0.6%Cu,0.05%~1.0%Bi,余量为Zr。合金元素优选范围为:0.8%~1.2%Nb,0.1%~0.4%Cu,0.1%~0.4%Bi。本发明的锆合金在400℃/10.3MPa过热蒸汽和360℃/18.6MPa去离子水中表现出优良的耐腐蚀性能,明显优于Zr-1Nb合金,且加工性好,可在核电站压水堆中用作燃料元件包壳以及定位格架条带等堆芯结构材料。

    核电站燃料包壳用含硫低Nb的锆锡铌合金

    公开(公告)号:CN103469010A

    公开(公告)日:2013-12-25

    申请号:CN201310398815.5

    申请日:2013-09-05

    Applicant: 上海大学

    CPC classification number: Y02E30/40

    Abstract: 本发明涉及一种能用作压水堆核电站燃料包壳以及定位格架条带等结构材料含硫的锆锡铌合金,属于锆合金材料技术领域。该锆合金的化学组成以重量百分比计为:0.3%~1.5%Sn,0.1%~0.59%Nb,0.1%~0.6%Fe,0~0.3%Cr,0.0005%~0.06%S,余量为Zr。合金元素优选范围为:0.5%~1.2%Sn,0.2%~0.5%Nb,0.2%~0.5%Fe,0~0.2%Cr,0.001%~0.05%S。本发明的锆合金在400℃过热蒸汽中均表现出优良的耐腐蚀性能,明显优于ZIRLO合金,可在核电站压水堆中用作燃料元件包壳以及定位格架条带等堆芯结构材料。