- Patent Title: High-strength steel pipe and producing method thereof
- Patent Title (中): 高强度钢管及其制造方法
-
Application No.: US13261070Application Date: 2010-06-10
-
Publication No.: US08685182B2Publication Date: 2014-04-01
- Inventor: Kensuke Nagai , Yasuhiro Shinohara , Shinya Sakamoto , Takuya Hara , Hitoshi Asahi
- Applicant: Kensuke Nagai , Yasuhiro Shinohara , Shinya Sakamoto , Takuya Hara , Hitoshi Asahi
- Applicant Address: JP Tokyo
- Assignee: Nippon Steel & Sumitomo Metal Corporation
- Current Assignee: Nippon Steel & Sumitomo Metal Corporation
- Current Assignee Address: JP Tokyo
- Agency: Kenyon & Kenyon LLP
- Priority: JP2009-140280 20090611
- International Application: PCT/JP2010/003866 WO 20100610
- International Announcement: WO2010/143433 WO 20101216
- Main IPC: C22C38/48
- IPC: C22C38/48 ; C22C38/50 ; C21D8/10

Abstract:
This high-strength steel pipe includes, by mass %, C: 0.02% to 0.09%, Mn: 0.4% to 2.5%, Cr: 0.1% to 1.0%, Ti: 0.005% to 0.03%, Nb: 0.005% to 0.3%, and a balance consisting of Fe and inevitable impurities, in which Si, Al, P, S, and N are limited to 0.6% or less, 0.1% or less, 0.02% or less, 0.005% or less, 0.008% or less, respectively, the bainite transformation index BT is 650° C. or less, and the microstructure thereof is a single bainite microstructure including first bainite and second bainite, the first bainite being a gathered microstructure of bainitic ferrite including no carbide, and the second bainite being a mixed microstructure of bainitic ferrite including no carbide and cementite between the bainitic ferrites.