Invention Grant
- Patent Title: Zirconia sintered body and production method the same
- Patent Title (中): 氧化锆烧结体和生产方法一样
-
Application No.: US12866701Application Date: 2009-02-06
-
Publication No.: US08383236B2Publication Date: 2013-02-26
- Inventor: Shunji Mikaki , Kunihide Shikata
- Applicant: Shunji Mikaki , Kunihide Shikata
- Applicant Address: JP Kyoto
- Assignee: Kyocera Corporation
- Current Assignee: Kyocera Corporation
- Current Assignee Address: JP Kyoto
- Agency: DLA Piper LLP (US)
- Priority: JP2008-027694 20080207
- International Application: PCT/JP2009/052054 WO 20090206
- International Announcement: WO2009/099184 WO 20090813
- Main IPC: B32B5/16
- IPC: B32B5/16

Abstract:
Provided are a zirconia sintered body that has excellent mechanical characteristics, as well as semiconductivity that can allow static electricity to escape at an appropriate rate, and a manufacturing method that can manufacture the same at lower cost than in the past. The zirconia sintered body is made of 66-90 parts by weight of zirconia that contains a stabilizer, and a total of 10-34 parts by weight of iron, chromium and titanium oxides. Of the iron, chromium and titanium oxides, the proportion of iron oxide is 70-99.5 wt %, the proportion of chromium oxide is 0.4-20 wt % and the proportion of titanium oxide is 0.1-10 wt %. The combined proportion of tetragonal and cubic crystals in the zirconia crystal phase is 90% or more and the mean crystal grain size of the zirconia is 0.3-0.5 μm. The mean crystal grain size of the iron, chromium and titanium oxides is 0.5-2.0 μm. It has excellent mechanical characteristics, as well as semiconductivity.