Invention Grant
US08236399B2 Lighter than air balloon made from a biaxially oriented polyester film
有权
比由双轴取向的聚酯薄膜制成的气球轻
- Patent Title: Lighter than air balloon made from a biaxially oriented polyester film
- Patent Title (中): 比由双轴取向的聚酯薄膜制成的气球轻
-
Application No.: US13196495Application Date: 2011-08-02
-
Publication No.: US08236399B2Publication Date: 2012-08-07
- Inventor: Gianfranco Chicarella , Nao Yokota , Tracy A. Paolilli , John J. Fitch , Todd Richard Sarnstrom , Dean Borchardt , Paul Andrew Ansolabehere , Steven Sargeant
- Applicant: Gianfranco Chicarella , Nao Yokota , Tracy A. Paolilli , John J. Fitch , Todd Richard Sarnstrom , Dean Borchardt , Paul Andrew Ansolabehere , Steven Sargeant
- Applicant Address: US RI North Kingstown US MN Eden Prairie
- Assignee: Toray Plastics (America), Inc.,Anagram International, Inc.
- Current Assignee: Toray Plastics (America), Inc.,Anagram International, Inc.
- Current Assignee Address: US RI North Kingstown US MN Eden Prairie
- Agency: Morrison & Foerster LLP
- Main IPC: B32B1/00
- IPC: B32B1/00 ; B32B1/08

Abstract:
A long life balloon formed from a lamination. The lamination includes a polyester film with a total thickness of 4 μm to 12 μm. The polyester film includes a biaxially oriented polyester core layer and at least one amorphous copolyester skin layer. The lamination also includes a sealant layer and a gas barrier layer on an opposite side of the polyester film from the sealant layer. The oxygen transmission rate of the balloon is less than 0.1 cc/100 sqin/day, a bonding strength of the gas barrier layer to the surface of the polyester film is more than 300 g/in at dry conditions, a sealing strength of the balloon is more than 3.5 kg/in, and a floating time of the balloon is more than 20 days.