Invention Grant
US07883817B2 Method for producing gas diffusion electrode and method for producing polymer electrolyte fuel cell, and gas diffusion electrode and polymer electrolyte fuel cell
有权
气体扩散电极的制造方法以及固体高分子型燃料电池的制造方法以及气体扩散电极和聚合物电解质型燃料电池
- Patent Title: Method for producing gas diffusion electrode and method for producing polymer electrolyte fuel cell, and gas diffusion electrode and polymer electrolyte fuel cell
- Patent Title (中): 气体扩散电极的制造方法以及固体高分子型燃料电池的制造方法以及气体扩散电极和聚合物电解质型燃料电池
-
Application No.: US11579344Application Date: 2005-07-05
-
Publication No.: US07883817B2Publication Date: 2011-02-08
- Inventor: Yoshihiro Hori , Mikiko Yoshimura , Yoichiro Tsuji , Takeshi Yonamine , Masaki Yamauchi
- Applicant: Yoshihiro Hori , Mikiko Yoshimura , Yoichiro Tsuji , Takeshi Yonamine , Masaki Yamauchi
- Applicant Address: JP Osaka JP Tokyo
- Assignee: Panasonic Corporation,Asahi Glass Co., Ltd.
- Current Assignee: Panasonic Corporation,Asahi Glass Co., Ltd.
- Current Assignee Address: JP Osaka JP Tokyo
- Agency: McDermott Will & Emery LLP
- Priority: JP2004-198916 20040706
- International Application: PCT/JP2005/012413 WO 20050705
- International Announcement: WO2006/004120 WO 20060112
- Main IPC: H01M8/10
- IPC: H01M8/10 ; H01M4/88 ; H01M4/96 ; H01M8/02

Abstract:
The present invention provides a gas diffusion electrode capable of sufficiently preventing not only degradation of MEA during storage but also degradation of initial characteristics and durability during the time period from production to initial use, and a polymer electrolyte fuel cell including the gas diffusion electrode. The gas diffusion electrode includes a catalyst layer in which A1 representing a total mass of organic substance comprising alcohol, a partial oxide of the alcohol, a product of intramolecular dehydrogenation reaction of the alcohol, a product of intermolecular condensation reaction of the alcohol, a product of intermolecular condensation reaction between the alcohol and the partial oxide and a product of intermolecular condensation reaction of the partial oxide, E1 representing a total mass of carbon powder and G1 representing a total mass of cation exchange resin are controlled to satisfy {100×A1/(E1+G1)}≦0.05.
Public/Granted literature
Information query