Surface modified cathode with improved lithium intercalation behavior
Abstract:
Surface modification of LiNi0.4Mn0.4Co0.2O2 (442) compound with certain inert (MxOy) metal oxides viz., Al2O3, Bi2O3, In2O3, Cr2O3, ZrO2, ZnO, MgO has been attempted with a view to improve the structural and cycling stability, especially upon high voltage and high rate cycling conditions. In addition to HF scavenging effect, the protective metal oxide inter-connect layer restricts the number of oxide ion vacancies eliminated during the initial cycling of cathode, resulting in the reduced irreversible capacity loss of the first cycle. Among the surface modified cathodes, Bi2O3 coated LiNi0.4Mn0.4Co0.2O2 cathode exhibits appreciable specific capacity values of 196 (Qdc1) and 175 (Qdc100) mAh g−1 with 89% capacity retention, thus evidencing the superiority of Bi2O3 modifier in improving the electrochemical behavior of pristine LiNi0.4Mn0.4Co0.2O2 cathode. Further, suitability of Bi2O3 coated LiNi0.4Mn0.4Co0.2O2 cathode for high voltage (5.0 V) and high rate (3 C) lithium intercalation and de-intercalation applications has been demonstrated up to 100 cycles.
Information query
Patent Agency Ranking
0/0